SYNTOWAX EO 110/10 (OPE10)
Polyethylene wax is oxidized.
It is delivered on pallets (1000 kg) in craft paper bags with a polyethylene liner of 20 kg.
Appearance |
Granules/Powder |
Drop point, °C, ASTM D127-08 |
70 – 100 |
Softening temperature, °C |
95 – 105 |
Acid value, mgKOH |
7 – 15 |
Penetration, 1/10мм, ASTM D1321 |
less than 11 |
Color |
white |
- Internal lubricant / lubricant, plasticizer for polymers (PVC, PP, HDPE, LDPE);
- The main component of wax emulsions;
- A component of various wax/paraffin compounds.
- Application
-
Application:
Micronized waxes are used as an additive in the production of coatings and surfaces, improving their gloss and glide, and they also contribute to good dispersion of resins and form a smooth layer on the surface to protect it from scratches and abrasion. They are part of powder and architectural paints, coatings for wood.
- Application
-
Application:
- External lubricant / lubricant, plasticizer for polymers (PVC, PP, HDPE, LDPE, Rubbers);
- Dispersant and plasticizer in super concentrates (masterbatches, polymer compositions);
- Viscosity regulator in hot melt adhesives and adhesives, oils, coolant;
- Component of wax compositions (paraffin compositions, model injection formulations for metallurgy, candles);
- Temperature and strength modifier in thermoplastics, bitumen.
- Application
-
Application
Advantages of the application:
- provides increased manufacturability and increased service life of the roadway;
- it forms a reinforcing spatial structure in the bitumen binder during cooling, which gives additional rigidity to the composition under operating load conditions;
- It has a positive effect on the number of penetrations, softening temperatures and adhesion to asphalt concrete filler;
- it increases the resistance against the displacement of the bitumen film from the rock surface with water, and also increases the resistance against chemical reagents;
- dispersion and dissolution in the binder is achieved at operating cooking temperatures of more than 110 C. The input can be carried out at the stage of preparation and processing of bitumen binder, with preliminary mechanical mixing with other fillers;
- The effectiveness is manifested when introducing up to 1.5% by weight into the binder.